95.00€ inc. VAT
3 in stock
Key features
Applications
Resin properties (uncured liquid)
Mechanical properties
Test method on post cured objects through 30 minutes high power LED curing.
| Properties | Typical Value | Test Method |
| Glass transition temperature (Tg) | 128°C | ASTM D7028 |
| Water absorption | 0.45% | ASTM D570-98 |
| Impact strength (IZOD notched) | 20 J/m | ASTM D256A |
| Tensile strength | 91 MPa | ASTM D638M |
| Tensile Modulus | 2500 MPa | ASTM D638M |
| Elongation at break | 8% | ASTM D638M |
| Flexural Strength | 135 MPa | ASTM D790M |
| Flexural Modulus | 3250 MPa | ASTM D2240 |
| Shore D Hardness | 87 | ASTM D2240 |
Please note that the above-displayed values can vary with individual machine processing, post-curing parts, geometry, print orientation, print settings, and temperature.
Preparation(s) before starting to print
Post-processing
We do advise you to post-process your 3D print in order to achieve the material properties
Safety
Please always be aware that when 3D printing with resins that you are working with chemicals and that you should always be cautious and use the personal protective equipment as stipulated in our safety data sheets.